1, High saturation magnetic induction
2, High permeability
3, Low coercivity
4, Excellent stability  
1,Made common mode chokes instead of Co-based amorphous,silicon steel sheet,ferrite,permalloy
2, Differential mode filter inductance  
3, High-frequency switching power supply  
4, High frequency inverter  
5, Zero-sequence current transformer, magnetic amplifier,etc.  
| Item | Numerical value | 
| Material Composition | FeCuNbSiB | 
| strip thickness tolerance(mm) | 32±2 | 
| Magnetic strength B800 | ≥1.2T | 
| Curie temperature(oC) | 570oC | 
| crystallization temperature | 500oC | 
| Saturation magnetostriction coefficient | <2×10-6 | 
| Initial permeability μi | ≥80000 | 
| Maximum permeability um | ≥500000 | 
| Density(g/cm³ ) | 7.2 | 
| electrical resistivity(μΩ.cm) | 130 | 
| Lamination factor | ≥0.8 | 
| Coercivity Hc | ≤1A/m | 
| Magnetic permeability μ (1kHz) | ≥70000 | 
| Magnetic permeability μ (10kHz) | ≥60000 | 
| Magnetic permeability μ (100kHz) | ≥10000 | 
| Operating Temperature Range | -50~120℃ | 
Inductance loss curve and the data
table at different frequencies

Typical Characteristic