| Parameter | Value | 
|---|---|
| Material Composition | FeCuNbSiB | 
| Thickness (um) | 28~35 | 
| Saturation Induction Bs (T) | 1.25 | 
| Curie Temperature (°C) | 570 | 
| Hardness Hv | 880 | 
| Crystalline Temperature Tc (°C) | 500 | 
| Saturation Magnetostriction | 2×10^-6 | 
| Initial Permeability μi | ≥80000 | 
| Maximum Permeability um | ≥500000 | 
| Density (g/cm³) | 7.2 | 
| Electrical Resistivity (μΩ.cm) | 130 | 
| Lamination Factor | ≥0.8 | 
| Operating Temperature Range | -50~120℃ | 
Our manufacturing process...
Our most efficient transformer cores are utilized in a variety of industries...
We offer comprehensive after-sales service...
We ensure careful and efficient transportation of our products...
The cores are constructed from high-permeability nano-crystalline materials...
They are ideal for high-frequency power transformers...
The role of wholesale most efficient transformer cores is pivotal in modern energy systems...
There is no picture description for this product